CAS Changchun Institute of Applied Chemistry co-develops rare earth isoprene rubber at 30.000 t level capacity

The Neodynium-based catalyst for isoprene polymerization is utilized to nearly 100 %. Polymerization time is less than 3 hrs, and cis-content of the rubber is over 97 %. Catalyst cost is lower than $ 800/to. The process is covered by 73 patents.

China Bio news release, January 13, 2014

Most popular posts:

This website stores cookies on your computer. These cookies are used to provide a more personalized experience and to track your whereabouts around our website in compliance with the European General Data Protection Regulation. If you decide to to opt-out of any future tracking, a cookie will be setup in your browser to remember this choice for one year.